Siab -kub GH2132 Alloy Tubing Rau Aero Cav
Qib: GH2132
Ntev: Customizable
Puab: Round, Square, Rectangular
Hom: Seamless
Raws li tus neeg muag khoom thiab chaw tsim khoom nyob rau hauv Suav teb, GNEE Steel muab nqi -nickel zoo- raws li cov khoom siv alloy.
- Xa E-mail:ss@gneesteel.com
- Tel:+8615824687445
Siab -kub GH2132 alloy tubing rau aero xyaw cov lus piav qhia

GNEE Siab -kub GH2132 alloy tubing rau aero xyaw
GH2132 (tseem hu ua A-286 lossis UNS S66286) alloy tubing yog hlau-raws li- kub alloy, tseem ceeb heev rau aero-engines vim nws qhov kev ua tau zoo nyob rau hauv qhov kub thiab txias. Nws yog tsim rau cov khoom uas xav tau lub zog siab, nkag siab, thiab oxidation kuj qis dua 650 degree.
GH2132 yog tsim los tswj lub zog ntawm qhov kub thiab txias, ua rau nws haum rau cov ntawv thov uas lwm cov ntaub ntawv tuaj yeem ua rau muaj zog tsawg. GH2132 nthuav tawm cov kev tiv thaiv zoo heev rau kev nkag mus deformation, uas yog qhov tseem ceeb rau cov ntaub ntawv raug kub thiab kub siab rau lub sijhawm ntev.
Specification Ntawm High -kub GH2132 alloy tubing rau aero xyaw
| Specifications ntawm High Temperature Gh2132 PIPES / TUBE: |
| Qib | Kub kub Gh2132 |
| Ntau yam | 1/2 "Nominal Bore rau 16" Nominal Bore |
| Ntev | Ib qho Random, Ob Chav Random & Txiav Ntev. |
| Ua kom tiav | Kub dov phaj (HR), Cold Rolled Sheet (CR), 2B, 2D, BA NO (8), SATIN (Met with Plastic Coated) |
| Daim ntawv | Round, Square, Rectangular, Hydraulic thiab lwm yam |
| Hom | Seamless / ERW / Welded / Fabricated / EFW |
| Daim ntawv thov | Tawm ntawm -Shore Roj Drilling tuam txhab, tsim hluav taws xob, Petrochemicals, Gas processing, Tshwj xeeb tshuaj, tshuaj, khoom siv tshuaj, tshuaj, khoom siv dej hiav txwv, tshav kub exchangers, condensers, pulp thiab ntawv kev lag luam |
Siab -kub GH2132 alloy tubing rau aero engine Specification
| CHEMICAL COMPOSITION NTAWMKub kub Gh2132: |
| Qib | C | Mn | Si | S | Cu | Fe | Ni | Cr |
| hwv 2132 | 0.08 max | max 2.00 Nws | 1.0 max | - | - | tshuav nyiaj li cas | 24-27.0 Nws | 13.5 – 16.00 |
Lub cev muaj zog ntawm GH2132 Pipe
| Khoom | Tus nqi |
|---|---|
| Qhov ntom | 7.93 g/m² |
| Melting Temperature Range | 1364-1424 degree |
| Modulus ntawm Elasticity | 196 gpa ua |
| Coefficient ntawm Thermal Expansion (20 degree) | 16.5 x 10^-6 / degree |
| Thermal conductivity | 11.3 W / m·K ntawm 100 degree |
| Tshwj xeeb kub muaj peev xwm | 502 J/kg · K |
| Hluav taws xob Resistivity | 0.85 µΩ·m |
Mechanical zog ntawm GH2132 Tube
| Khoom | Tus nqi |
|---|---|
| Yield zog (Rp0.2) | 665 MPa ua |
| Tensile zog (Rm) | 943mpa ua |
| Elongation (A) | 13% |
| Kev txo qis hauv cheeb tsam (Z) | 22% |
| Brinell Hardness (HBW) | 422 |
Daim ntawv thov ntawm High-kub GH2132 alloy tubing rau aero xyaw
Aero Engine Applications
GH2132 alloy tubing yog siv nyob rau hauv ntau yam tseem ceeb siab -kub bearing Cheebtsam hauv aero engines, suav nrog:
Hydraulic thiab pneumatic tswj systems
Thaum tshav kub kub exchangers
Combustion Chamber Cheebtsam
Cov khoom siv xws li kev txhawb nqa cov qauv thiab cov casings
Thaum GH2132 alloy tubing kuj tseem siv rau hauv lwm cov khoom xws li turbine blades thiab turbine disks, feem ntau yog siv rau hauv cov koom haum pabcuam vim tias nws tuaj yeem tiv taus siab, kub hloov pauv, thiab kev co, thaum tseem ua rau lub teeb yuag.
Siab -kub GH2132 alloy tubing rau aero xyaw cov txheej txheem tsim khoom
Gnee Steel muab cov kev kho cua sov hauv qab no rauSiab -kub GH2132 alloy tubing rau aero xyaw: annealing, tov + laus. Tsis tas li ntawd, Gnee Steel tseem muab kev ua haujlwm kub thiab txias ua haujlwm, uas yog kub dov thiab kos duab txias.
Siab -kub GH2132 alloy tubing rau aero engine Ntim
1. Kev ntim khoom yog qhov tseem ceeb, tshwj xeeb tshaj yog nyob rau hauv kev xa khoom thoob ntiaj teb, qhov twg cov khoom tau dhau los ua ntau theem kom ncav cuag lawv qhov chaw kawg; yog li ntawd, peb muab qhov tseem ceeb ntawm kev ntim khoom.
2. Gnee Steel siv ntau txoj kev ntim khoom nyob ntawm cov khoom. Piv txwv li, peb siv ntau txoj kev ntim khoom ...
Hais txog Gnee Steel

Gnee Steel tshwj xeeb hauv kev tsim thiab muag ntawm ntau yam nickel-raws li alloys, suav nrog Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 71, Inconel Alloy 800, Incoloy 800H / HT, Incoloy 825, Monel Alloy 400, Monel K500, thiab kub kub alloys. Gnee Steel cov khoom siv dav siv hauv aerospace, tshuaj, hluav taws xob, tsheb, thiab kev siv hluav taws xob nuclear. Peb kuj muab cov kev daws teeb meem customized alloy raws li cov neeg siv khoom xav tau. Rau cov lus nug txog tus nqi alloy lossis customized alloy kev daws teeb meem, thov hu rau peb rau kev tsocai ntawmss@gneesteel.com.
Cim npe nrov: siab-kub gh2132 alloy tubing rau aero xyaw, Tuam Tshoj siab-kub gh2132 alloy tubing rau aero xyaw lwm tus neeg