GH3030 Pipe Description

GNEE GH3030 Tube
GH3030 yog nickel-chromium-raws li cov khoom siv tshuaj ntxiv dag zog rau superalloy tsim los rau cov ntawv thov uas yuav tsum tau muaj kev tiv thaiv oxidation zoo thiab kev ua haujlwm ruaj khov ntawm qhov kub thiab txias. GH3030 steel yeeb nkab yog thoob ntiaj teb lees paub tias yog qhov sib npaug rau Nimonic 75, tswj cov khoom zoo heev hauv oxidizing cua ntawm qhov kub txog li 800℃(nruam) thiab 1000℃(lub sijhawm luv).
Gnee Steel, ib lub chaw tsim khoom ntawm superalloys, muaj GH3030 steel yeeb nkab nrog cov qauv zoo tshaj plaws, ua kom pom kev ua haujlwm zoo hauv cov chav sib txuas, cov khoom siv hluav taws xob, thiab cov cub tawg.
Nrhiav rau ib tug txhim khu kev qha muab saw hlau khub? Peb muab cov nqi lag luam wholesale nqe rau GH3030 yeeb nkab xaj.
Tau txais daim ntawv tsocai rau GH3030 yeeb nkab tam sim no
| IB QHOV CHAW UA HAUJ LWM ntawm Kub Kub Gh3030: |
| Tuam Tshoj | Kazakhstan |
| GH3030 | XH78T |
Dimensions & Available Size Range
Peb tshwj xeeb hauvPrecision Cold Drawn & Bright Annealedtubing nrog nruj tolerances.
Sab nraud txoj kab uas hla (OD):6.0mm-219.0 hli
Phab ntsa Thickness (WT):0.5mm-20.0 hli
Ntev:Standard 6m los yogPrecision Txiav-rau-Length(± 1 hli).
Nto tiav: Bright Annealed (BA), Pickled, los yogPolished(rau koj cov cai Ra).



Alloy GH3030 Yeeb Nkab Specifications
| Specifications ntawm High Temperature Gh3030 PIPES / TUBE: |
| Qib | Kub kub Gh3030 |
| Ntau yam | 1/2 "Nominal Bore rau 16" Nominal Bore |
| Ntev | Ib qho Random, Ob Chav Random & Txiav Ntev. |
| Ua kom tiav | Kub dov phaj (HR), Cold Rolled Sheet (CR), 2B, 2D, BA NO (8), SATIN (Met with Plastic Coated) |
| Daim ntawv | Round, Square, Rectangular, Hydraulic thiab lwm yam |
| Hom | Seamless / ERW / Welded / Fabricated / EFW |
GH3030 yeeb nkab Seamless yeeb nkabSpecification
Tshuaj muaj pes tsawg leeg (%) ntawm GH3030 yeeb nkab
Peb GH3030 nruj me ntsis raws li GB / T 15062 thiab aerospace-qib cov qauv.
| Element | Ni | Cr | Ti | Al | Fe | C | Mn | Si | P | S |
| Min | Bal | 19.00 | 0.15 | - | - | - | - | - | - | - |
| Max | Bal | 22.00 | 0.35 | 0.15 | 1.50 | 0.12 | 0.70 | 0.80 | 0.015 | 0.010 |
Mechanical zog ntawm GH3030 yeeb nkab (ntawm chav tsev kub)
| Khoom | Tus nqi |
|---|---|
| Tensile zog (Rm) | Ntau dua lossis sib npaug li 590 MPa |
| Yield zog (Rp0.2) | Ntau dua lossis sib npaug li 245 MPa |
| Elongation (A5) | Ntau dua lossis sib npaug li 35% |
| Hardness | Tsawg dua lossis sib npaug li 200 HBW |
GH3030 Pipe - Lub cev muaj zog
| Lub cev khoom | Tus nqi |
|---|---|
| Qhov ntom | 8.4 g / cm³ |
| Melting Range | 1374℃- 1420 degree |
| Tshwj xeeb kub (20-100 degree) | 440 J / (kg·K) |
GH3030 Seamless Tube: Loj & Theoretical Luj Daim Ntawv Qhia

Qhov hnyav theoretical yog xam raws li GH3030 ntom ntawm8.4 g / cm³.
Formula: Nyhav (kg/m )=(OD - WT) × WT × 0.02638
| Sab nraud Diameter (OD) | Phab ntsa Thickness (WT) | Qhov hnyav (kg / m) | Kev Ua Haujlwm |
| 6.0 mm | 1.0 mm | 0.132 kg | Cold Drawn / Capillary |
| 10.0 mm | 1.5 mm | 0.336 kg | Txias Drawn |
| 18.0 mm | 2.0 mm | 0.844 kg | Cold Drawn / BA |
| 25.0 mm | 2.5 mm | 1.484 kg | Txias Drawn |
| 38.0 mm | 3.0 mm | 2.770 kg | Cold Drawn / Kub Rolled |
| 57.0 mm | 3.5 mm | 4.945 kg | Kub Rolled / Pickled |
| 76.0 mm | 4.0 mm | 7.597 kg | Kub Rolled |
| 108.0 mm | 5.0 mm | 13.586 kg | Kub Rolled / Forged |
| 219.0 mm | 8.0 mm | 44.530 kg | Forged & Machined |
2. GH3030 kwv yees tso cai rau siab ntsuas lub rooj
Cov kev ntsuas siab tau suav nrog cov qauv Barlow thiab suav nrog tus qauv kev nyab xeeb. Raws li cov kws paub txog qhov kub thiab txias, Gnee Steel sau tseg tias qhov kev tso cai siab txo qis qis thaum ua haujlwm kub nce.
Khoom siv: Annealed GH3030 Seamless Tube
| OD x WT (mm) | ntawm 20℃(MPa) | ntawm 600℃(MPa) | ntawm 800℃(MPa) |
| 10 x 1.0 | 25.5 MPa | 17.8 MPa | 8.2 MPa |
| 18 x 1.5 | 21.2 MPa | 14.8 MPa | 6.8 MPa |
| 25 x 2.0 | 20.4 MPa | 14.2 MPa | 6.5 MPa |
| 38 x 3.0 | 20.0 MPa | 14.0 MPa | 6.4 MPa |
| 57 x 4.0 | 17.9 MPa | 12.5 MPa | 5.7 MPa |
| 76 x 5.0 | 16.7 MPa | 11.6 MPa | 5.3 MPa |
| 108 x 6.0 | 14.2 MPa | 9.9 MPa | 4.5 MPa |
Tsis lees paub:Cov duab no yog rau kev siv engineering nkaus xwb. Cov kev txwv siab tiag tiag yuav tsum coj mus rau hauv tus account qhov kev tiv thaiv corrosion thiab cov qauv kev nyab xeeb tshwj xeeb (ASME, GB, lossis EN).
3. Cov Qauv Tseem Ceeb rau GH3030 Cov kav dej
Peb muab GH3030 tubing nrog qhov siab qhov tseeb kom paub meej seamless sib dhos hauv koj cov roj manifold lossis cov khoom siv hluav taws xob.
Sab nraud Diameter (OD) kam rau ua:± 0.1% lossis ± 0.05 hli (qhov twg yog qhov nruj dua).
Phab ntsa Thickness (WT) kam rau ua:± 10% lossis ± 0.03 hli.
Kev ncaj:Tsawg dua lossis sib npaug li 1.0 hli ib 'meter' (rau cov tshuab pub mis tsis siv neeg).
Daim ntawv thov ntawmGH3030 cev& Tube
GH3030 cevyog ib qho tseem ceeb tivthaiv rau qhov chaw uas raug thermal cycling:
Aerospace:Roj tubing thiab nplaim hluav taws nyob rau hauv dav hlau cav combustion chambers.
Muaj Furnaces:Radiant tubes, thermocouple sheaths, thiab rauv hauv ob sab phlu.
Kev tsim hluav taws xob:Internal piping rau high-temperature chav thiab roj turbines.
Petrochemicals:Catalyst txhawb cov raj thiab cov cua kub kub exchangers.






Kev Xeem NtawmGH3030 Alloy yeeb nkab
Gnee Steel muaj npe nrov rau nws qhov zoo meej qhov tseeb. Tag nrho cov khoom raug kuaj nruj ua ntej xa zaub mov. Peb ua ob qho tib si kev puas tsuaj thiab tsis muaj kev puas tsuaj rau txhua yam khoom.
Eddy kev sim tam sim no
Hydrostatic siab tsom xam
Pitting corrosion tiv thaiv kev kuaj
Lub zog tsim kev lag luam
Kev txheeb xyuas cov khoom muaj pes tsawg leeg
GH3030 seamlessYeeb Nkab Ntim
Gnee Steelsiv txoj kev ntim khoom zoo tshaj plaws thiab zoo tshaj plaws rau txhua hom kev thauj mus los. Peb txoj kev ntim khoom muaj xws li:
Ntoo crates
Ntoo pallets
Shrink wrap packing
Cardboard thawv
Ntoo crates
Hais txog Gnee Steel

Txhawm rau kom ntseeg tau xoom-tsis muaj kev ntseeg siab nyob rau hauv high-speed airflow ib puag ncig, txhuaGH3030 cevundergoes ib tug nruj zoo tswj txheej txheem:
Nqus Induction Melting + Electroslag Remelting:Nqus induction melting ua ke nrog electroslag remelting yields ultra-ntshiab hlau.
Txias Rolling/Drawing:Multi-pass processing ua tiav qhov tseeb qhov tseeb.
Bright Annealing:Annealing yog ua nyob rau hauv ib qho chaw tswj hydrogen kom huv si, scale-dawb nto.
100% Kev Ntsuas Tsis Muaj Kev Ua Phem:Txhua cov yeeb nkab tau dhau qhov kev sim tam sim no thiab kuaj ultrasonic (UT).
Ntawv pov thawj:Tag nrho cov khoom xa tuaj tuaj nrog ua tiav EN 10204 3.1 Material Testing Certificate (MTC).




Gnee Steel GH3030 Tube daim ntawv pov thawj
FAQ
Q1: GH3030 piv rau 310S Stainless Steel kav li cas?
A:Thaum 310S yog cov hlau uas tsis muaj cua sov, GH3030 yog nickel-based superalloy. Nws muaj qhov ua tau zoo dua oxidation tsis kam thiab tiv thaiv "sigma theem" embrittlement uas cuam tshuam rau cov hlau tsis muaj steel tom qab ntev raug rau 800 degree.
Q2: Cov raj GH3030 puas tuaj yeem yooj yim welded?
A:Yog lawm. GH3030 yog khoom plig rau nws zoo heev weldability. Nws tuaj yeem koom nrog siv TIG, MIG, lossis qhov chaw vuam yam tsis muaj kev pheej hmoo ntawm kev sib tsoo tom qab vuam, ua rau nws zoo tagnrho rau cov txheej txheem thermal.
Q3: Dab tsi yog koj lub sij hawm ua cov khoom siv rau cov raj me me?
A:Cov khoom lag luam xa tuaj rau hauv7 days. Rau kev txiav txim-draw precision txiav txim, peb lub sij hawm coj mus kuaj yog3 mus rau 4 hnub, suav nrog tag nrho cov kev sim tsis muaj kev puas tsuaj.
Q4: Koj puas txhawb nqa thoob ntiaj teb qhov rooj rau qhov rooj xa khoom?
A:Yog lawm. Raws li kev paubntiaj teb no exporter, peb muab huab cua, hiav txwv, thiab nthuav qhia logistics nrog tag nrho cov kev lis kev cai clearance txhawb rau ntau tshaj 60 lub teb chaws.
Cim npe nrov: gh3030 yeeb nkab, Tuam Tshoj gh3030 yeeb nkab lwm tus neeg
Tom ntej
GH 3030 BarKoj Tseem Yuav Zoo Li
Xa kev nug