GH3536 Alloy Bar
video

GH3536 Alloy Bar

GH3536 yog Ni-Cr-Fe-raws li cov khoom siv ntxiv dag zog deformed high-temperature alloy. Thaum siv hauv casting, cov qib sib thooj yog K4536. Lub alloy muaj nruab nrab durability thiab creep zog hauv qab 900 degree; nws muaj oxidation zoo thiab corrosion kuj, zoo kub thiab txias ua formability thiab vuam kev ua tau zoo.
Xa kev nug
Tsham tam sim no

Raws li tus neeg muag khoom thiab chaw tsim khoom nyob rau hauv Suav teb, GNEE Steel muab tus nqi -nickel zoo- raws li cov khoom siv alloy.

Khoom Taw qhia

hwv 3536(tseem hu uaHastelloy X) yog cov nickel-based superalloy ntxiv dag zog los ntawm cov khoom siv ntawm Cr thiab Mo cov ntsiab lus, uas yog siv dav hauv cov roj turbine xyaw thiab petrochemical reactors vim nws qhov kub thiab txias zog, toughness thiab corrosion kuj. Feem ntau GH3536 alloys yog siv nyob rau hauv huab cua huab cua huab cua nrog kub siab, siab oxidation degree thiab lub sij hawm ntev thermal cycling.

Tshuaj muaj pes tsawg leeg (wt.%) ntawm GH 3536

Cov ntsiab lus Min.(Ntau dua lossis sib npaug) Max.(Less tshaj los yog sib npaug)
Ni - Bal
Cr 20.50 23.50
Fe 17.00 20.00
C 0.05 0.15
Mn - 1.00
Si - 1.00
Mo 8.00 10.00
Co 0.50 2.50
Al - 0.10
W 0.20 1.00
B - 0.005
P - 0.015
S - 0.01

Mechanical Properties ntawm GH 3536

Rp0.2(MPa) Rm(MPa) Kev cuam tshuam
KV (J)
Elongation
A (%)
A Z (%) Kev xa khoom Hardness HB
155 (Ntau dua lossis sib npaug) 542 (Ntau dua lossis sib npaug) 33 21 23 Solution & Aging, Ann, Ausaging, Q+T 432

Super Alloy

GH3536 Alloy Mechanical zog

1. Tensile zog:Ntawm chav tsev kub, lub zog tensile ntawm GH3536 tuaj yeem ncav cuag li 1000 MPa. Raws li qhov kub thiab txias, nws lub zog tensile yuav txo qis, tab sis nws tseem tuaj yeem tswj tau lub zog siab.

2. Yield zog:Lub zog tawm los ntawm GH3536 kuj yog siab heev, ncav cuag ntau tshaj 500 MPa ntawm chav tsev kub. Qhov no muab cov hlau zoo yas deformation muaj peev xwm thaum raug thauj khoom.

3. Elongation:Ntawm chav tsev kub, qhov elongation ntawm GH3536 tuaj yeem ncav cuag ntau dua 15%. Qhov no qhia tau hais tias lub alloy muaj peev xwm mus undergo loj yas deformation thaum raug tensile kev nyuaj siab, yog li txhim kho nws puas toughness.

superalloy GH3536 Thaum tshav kub kub kuj

GH3536 Superalloy muaj cov cua sov ua haujlwm zoo thiab tuaj yeem ua haujlwm tau ntev hauv qhov kub thiab txias yam tsis muaj kev ua haujlwm tsis zoo. Nws cov hluav taws kub tsis kam yog feem ntau cuam tshuam hauv oxidation tsis kam, corrosion kuj thiab creep kuj. Nyob rau hauv qhov kub thiab txias oxidation ib puag ncig, GH3536 tuaj yeem tsim cov oxide zaj duab xis kom zoo tiv thaiv cov hlau matrix los ntawm kev oxidation ntxiv; nyob rau hauv qhov kub thiab txias ib puag ncig corrosion, lub alloy kuj qhia tau hais tias zoo corrosion kuj; Nyob rau hauv qhov kub thiab txias creep tej yam kev mob, GH3536 muaj ib tug tsawg creep tus nqi thiab muaj peev xwm tswj kom zoo seem stability.