Ams 5661 / USN N09901 superalallo sawb rau dav hlau tshuab incoloy 901 npib tsib xee alloy chev
Incoloy 901 daim ntawv thov ▪ Cov dav hlau cav ▪ Lub tsev dav hlau ▪ Cov dav hlau lub tshuab hluav taws xob ▪ Tus lej ▪ "▪ ACH ANE 5661 ▪ ISOH 9725 ▪ MSRR 7029, MSRR 7031 ▪ Nimonic Alloy 901 Incoloy ...
Xa kev nug
Tsham tam sim no
Raws li tus neeg muag khoom thiab chaw tsim khoom nyob rau hauv Suav teb, GNEE Steel muab tus nqi -nickel zoo- raws li cov khoom siv alloy.
- Xa E-mail:ss@gneesteel.com
- Tel:+8615824687445
Khoom Taw qhia
Incoloy 901 Daim Ntawv Thov
▪ Roj tshuab
Aircraft cav
▪ Turbine OF Ring
Tus Thawj Coj
Incoloy 901 specifications
▪ Tsis yog N09901
▪ Tus lej Werkstoff 2.4662
Br HR HR 55
▪ Ams 5660
▪ Ams 5661
▪ AECMA PREN2176
▪ AECMA PREN2177
▪ ISO 9723
▪ ISO 9725
MSRR 7029, MSRR 7031
▪ Nimonic alloy 901
Incoloy 901Tshuaj Muaj Tshuaj
| Lub ntsiab | Cov ntsiab lus (%) |
| Npib tsib xee, ni | 40-45 |
| Hlau, FE | 33 |
| Chromium, cr | 11-14 |
| Molybdenum, mo | 5.0 - 6.50 |
| Titanium, ti | 2.80-3.10 |
| Cobalt, CO | 1 |
| Manganese, mn | 0.50 |
| Tooj liab, cu | 0.50 |
| Silicon, si | 0.40 |
| Aluminium, al | 0.35 |
| Carbon, c | 0.10 |
| Sulphur, s | 0.030 |
Incoloy 901Cov Khoom Siv Neeg Kho Tshuab
| Cov Khoom Siv | Me me | Muaj huab tais |
| Tensile lub zog (nag tes nyuaj, muaj nuj nqis ntawm chav tsev kub) | 1200 MPa | 174000 psi |
| Peple Zog (@Strain 0.200%, Zej Zog Ntaus tawv, muaj nuj nqis ntawm chav tsev kub) | 875 MPa | 127000 psi |
| Elongation thaum so (daus daus tawv tawv) | 15% | 15% |