GH1140 Alloy Bar
video

GH1140 Alloy Bar

GH1140 yog ib qho kev daws teeb meem ntxiv dag zog rau cov hlau-nickel-based superalloy, ntxiv rau ntau cov chromium, thiab nrog ib qho me me ntawm tungsten, molybdenum, aluminium thiab titanium thiab lwm yam khoom los ntxiv dag zog rau cov khoom siv.
Xa kev nug
Tsham tam sim no

Raws li tus neeg muag khoom thiab chaw tsim khoom nyob rau hauv Suav teb, GNEE Steel muab tus nqi -nickel zoo- raws li cov khoom siv alloy.

Khoom Taw qhia

HWV 1140alloy yog ib tug high-performance npib tsib xee-raws li alloy, feem ntau yog raws li nickel thiab chromium, uas yog feem ntau siv nyob rau hauv daim ntawv thov uas yuav tsum tau zoo kub-kub khoom thiab machinability. Nws yog ib qho tseem ceeb heev nyob rau hauv kev lag luam kev siv, tshwj xeeb tshaj yog nyob rau hauv cov kub kub, corrosion kuj thiab zoo mechanical zog yuav tsum tau.Lub ntsiab Cheebtsam ntawm GH1140 alloy muaj xws li npib tsib xee thiab chromium, thiab tej zaum kuj muaj lwm yam xws li hlau, molybdenum thiab titanium. , uas ua ke muab cov alloy zoo heev kub thiab zoo mechanical zog. Qhov piv ntawm npib tsib xee rau chromium thiab qhov sib ntxiv ntawm lwm cov ntsiab lus alloying ua lub luag haujlwm txiav txim siab hauv tag nrho cov khoom ntawm cov hlau.

GH1140 Tshuaj muaj pes tsawg leeg

keeb

C

Cr

Hauv

IN

Mo

Al

Ntawm

Loj feem /%

0.06-0.12

20.00-23.00

35.00-40.00

1.40-1.80

2.00-2.50

0.20-0.60

0.70-1.20

keeb

Fe

Qhov no

Mn

Thiab

P

S

 

Loj feem /%

Nyob twj ywm

Tsawg dua lossis sib npaug rau 0.050

Tsawg dua lossis sib npaug rau 0.70

Tsawg dua lossis sib npaug rau 0.80

Tsawg dua lossis sib npaug rau 0.025

Tsawg dua lossis sib npaug rau 0.015

 

GH1140 lub cev thiab txhua yam khoom

ceev

Melting point

8.09 g / cm³

-

super alloy metals GH1140

GH1140 Bar nta

GH1140 alloy pas nrig muaj cov txheej txheem kev ua tau zoo thiab tuaj yeem ua haujlwm kub thiab ua haujlwm txias. Nyob rau hauv cov nqe lus ntawm kev kub ua, cov hlau muaj zoo plasticity thiab tuaj yeem tiv taus ntau yam txheej txheem kub, xws li casting, forging, vuam, thiab lwm yam. Nyob rau hauv cov nqe lus ntawm kev ua txias, cov hlau yuav dov, kos, stamped thiab lwm yam txheej txheem kom tau cov khoom. ntawm ntau yam duab thiab specifications.

daim ntawv thov ntawm superalloy gH1140 bar

Vim qhov kev ua tau zoo ntawm qhov kub thiab txias tsis kam ntawm GH1140 alloy pas nrig, nws yog dav siv hauv aviation, aerospace, lub zog thiab lwm yam. Hauv kev lag luam aviation, cov hlau tuaj yeem siv los tsim cov khoom kub ntawm aerospace xyaw, xws li combustion chambers, turbine blades, thiab lwm yam; nyob rau hauv aerospace teb, cov hlau yuav siv tau los tsim kub qhov chaw ntawm foob pob ua ntxaij cav, xws li nozzles, combustion chambers, thiab lwm yam .; nyob rau hauv lub zog teb, lub alloy yuav siv tau los tsim cov khoom nyob rau hauv high kub reactors, xws li roj rods, tswj rods, thiab lwm yam.

Ntim & Shipping

sss super alloys GH1140

Cim npe nrov: gh1140 alloy bar, Tuam Tshoj gh1140 alloy bar lwm tus neeg