GH4169 alloy
Raws li tus neeg muag khoom thiab chaw tsim khoom nyob rau hauv Suav teb, GNEE Steel muab tus nqi -nickel zoo- raws li cov khoom siv alloy.
- Xa E-mail:ss@gneesteel.com
- Tel:+8615824687445
GH4169 yog Fe-Ni-Cr-raws li nag lossis daus hardening deformation superalloy. Kev siv lub sijhawm ntev kub yog -253 ~ 650 degree, thiab lub sijhawm siv sijhawm luv yog 800 degree . Nws muaj lub zog siab, zoo toughness thiab zoo toughness nyob rau hauv siab thiab qis kub ib puag ncig nyob rau hauv 650 degree. Nws yog resistant rau oxidation thiab corrosion. Thiab kev ua tau zoo ntawm kev ua tau zoo thiab vuam kev ua tau zoo thiab kev ua haujlwm ntev ntev. Nws tuaj yeem tsim ntau yam nrog cov duab nyuaj, thiab tau siv dav hauv qhov ntsuas kub saum toj no hauv aerospace, nuclear zog, roj av kev lag luam thiab extrusion tuag.
Tom ntej: Superalloy GH4169Thermal conductivity
| θ / degree | 11 | 100 | 200 | 300 | 400 | 500 | 600 | 700 | 800 | 900 | 1000 |
| λ/(W/(m•C)) | 13.4 | 14.7 | 15.7 | 17.8 | 18.3 | 19.6 | 21.2 | 22.8 | 23.6 | 27.6 | 30.4 |
Cov alloy GH4169 linear expansion coefficient
| θ / degree | 20~100 | 20~200 | 20~300 | 20~400 | 20~500 | 20~600 | 20~700 | 20~800 | 20~900 | 20~1000 |
| /10-6C-1 | 11.8 | 13.0 | 13.5 | 14.1 | 14.4 | 14.8 | 15.4 | 17.0 | 18.4 | 18.7 |
GH4169 tshwj xeeb tshav kub muaj peev xwm
| θ / degree | 300 | 400 | 500 | 600 | 700 | 800 | 900 | 1000 |
| c/(J/(kg·C)) | 481.4 | 493.9 | 514.8 | 539.0 | 573.4 | 615.3 | 657.2 | 707.4 |

GH4169 alloy kev ua tau zoo
Vim muaj cov ntsiab lus niobium siab hauv GH4169 alloy, niobium segregation Cheebtsam hauv cov hlau yog ncaj qha ntsig txog cov txheej txheem metallurgical. Lub melting ceev ntawm electroslag remelting thiab nqus arc melting thiab qhov zoo ntawm electrode qws ncaj qha cuam tshuam rau qhov zoo ntawm cov khoom. Ceev ceev melting yog ib qho yooj yim los tsim niobium-nplua nuj dub me ntsis; qeeb melting ceev yuav tsim niobium-poob dawb me ntsis; qhov tsis zoo ntawm cov electrode pas nrig thiab cov kab nrib pleb hauv cov pas nrig electrode yog ib qho yooj yim los ua kom muaj cov pob dawb. Yog li ntawd, kev txhim kho qhov zoo ntawm cov electrode pas nrig, tswj lub melting ceev thiab nce lub solidification tus nqi ntawm cov ingot yog ib qho tseem ceeb ntawm cov txheej txheem smelting.
Cov chaw thov ntawm GH4169 suav nrog:
GH4169 tuaj yeem siv dav hauv ntau lub sijhawm xav tau:
1. Chav turbine
2. Lub foob pob hluav taws ua kua
3. Cryogenic engineering
4. Acid ib puag ncig
5. Nuclear engineering