Alloy 4130 steel vuam yeeb nkab
video

Alloy 4130 steel vuam yeeb nkab

4130 Chromoly Tubing Qhov Ntau

Sab nraud txoj kab uas hla: 1 / 2 -1-1 / 2 "
Phab Ntsa Thickness: .065 - .120 "
Ntev: Upto 288 "
Pib: 5 txog 80s
Xa kev nug
Tsham tam sim no

Raws li tus neeg muag khoom thiab chaw tsim khoom nyob rau hauv Suav teb, GNEE Steel muab tus nqi -nickel zoo- raws li cov khoom siv alloy.

Khoom Taw qhia

Gnee Alloy 4130 Vuam Yeeb Nkab Qhia

4130 steel vuam yeeb nkab

Alloy 4130 steel welding PipeAlloy 4130 steel welding Pipe

4130 Alloy Steel Welded Tube (4130 chromoly welded Tube-molybdenum}) los ntawm high-furding (}} Kev khwv nyiaj txiag {{} lub raj welded muaj lub zog loj dua lossis muaj txiaj ntsig ntawm 1015g ntawm 720mpa ntau dua los yog muaj txiaj ntsig zoo dua lossis muaj txiaj ntsig ntawm 7,666 Kuj muaj cov yeeb nkab siv hluav taws xob ntau dua 90%, thiab muaj peev xwm ua tau zoo dua li 90%), thiab muaj peev xwm ua kom muaj txiaj ntsig zoo dua li 90% 1-20 mm. Nws yog cov khoom siv thauj khoom zoo li no (cov khoom thauj Epoxy txheej, thiab cov kev cuam tshuam hluav taws xob tseem tuaj yeem raug tswj hwm kom tau zoo rau ib puag ncig roj thiab tsis muaj kev kho mob hauv qab ntawm cov neeg siv hluav taws xob siab Thaj Tsam . Nrog nws cov kev xaiv zoo tshaj plaws, ua kom muaj kev xaiv zoo nkauj rau kev ntsuas qhov kev ua tau zoo thiab cov nuj nqis hauv cov teb txua.

Gnee Alloy 4130 Hlau Yeeb Nkab Tshwj Xeeb

4130 Chromoly Welded Hlau Tubing Kev Tshwj Xeeb

Cov cuab yeej qeb Cov ncauj lus kom ntxaws / Cov lus piav qhia
Txheem Qhov Dimension Od (hli):10 - 800 (Customizable)
Phab ntsa tuab (hli): 1.0 – 20.0
Ntev (m):6 (Txuj Ci), Max 18 (Kev Cai)
Tswj qauv - ASTM A513 (hluav taws xob-ua haujlwm welded)
- ASTM A787 (SSAWW / HFW HLES)
- EN 10219 (EU Welded)
- JIS G3445 (Nyiv)
Vuam txheej txheem ⚡️ Hlob/ Hfw/ Txiav ntoo
Nco tseg: erw feem ntau rau cov qauv hlab
Nto Kho - Raws li-welded + pickling(tshem oxide)
- Leeg Sib Tsoo(Weld Bead Tshem Tawm)
- Galvanized(kub-dip / zinc plating)
- Hmoov txheej(Siv)
Kev nyuaj - Cov khoom siv hauv paus (Q & T):25-32 hrc
- Kev kub siab (thaj tsam kub txwv):± 10% sib txawv
Annealed xeev: tsawg dua los yog sib npaug rau 220 HB
Ceev 7.85 g / cm³
Cov Khoom Siv Cov Khoom Siv Ib astm A513:
- C: 0.28-0.33%
- CR: {0.80-1.10%
- Mo: 0.15-0.25%
- s / p tsawg dua lossis sib npaug rau 0.040% (↑ vs seamless)
Cov Khoom Siv Neeg Kho Tshuab Tom qab weld kho cua sov (pwht):
- tensile lub zog: ntau dua lossis sib npaug zos rau 620 mpa
- Tawm lub zog: ntau dua los yog sib npaug rau 415 MPa
- elongation: ntau dua los yog sib npaug rau 10%
Thawj cov ntawv thov Nyem:Trailer thav ntawv, forklift masters
Kev Tsim Kho:Scaffolding, Txheej Txheem Trusses
Ua Liaj Ua Teb:Cov tshuab luam ntawv tshuab
Rooj tog:High-zog racks, cov khoom siv gym

4130 PIPES tshuaj muaj pes tsawg leeg:

Teem nqi C Si Mn S P Cr Ni Mo
4130 0.28-0.33 0.15-0.35 0.4-0.6 0.025 0.035 0.08-1.10 0.50 0.15-0.25

Gnee 4130 Vuam Yeeb Nkab Sij Hawm

4130 Welded Yeeb Nkab Daim Ntawv Qhia

Qhov loj Tus id Od Phab Ntsa Thickness
1 1.049 1.315 0.133
3/4 0.824 1.05 0.113
1 1/4 1.380 1.66 0.140
2 2.157 2.375 0.109
1 1/2 1.610 1.90 0.145
2 1/2 2.635 2.875 0.120
1/2 0.622 0.84 0.109
3 1/2 3.760 4.0 0.120
3 3.260 3.50 0.120
4 4.260 4.5 0.120
6 6.407 6.625 0.109
5 5.187 5.563 0.188

Gnee Pab Pawg Hoobkas Ib puag ncig

Gnee Group Alloy 4130 Yeeb Nkab Lub Tshuab Hluav Taws Xob

Alloy 4130 steel welding Pipe

Gnee Pab Pawg 4130 Ntim Ntim

Gnee Pab Pawg Chromoly Alloy 4130 tus Hlau Vuam Yeeb Ntim

Alloy 4130 steel welding Pipe

Gnee Pab Pawg Kev Ntsuas

Gnee Pab Pawg Chromoly 4130 Hlau Vuam Yeeb Kev Kuaj

Alloy 4130 steel welding Pipe

Cov FAQ

1. Dab tsi yog 4130 chrome-molybdenum hlau siv rau?
4130 chrome-molybdenum hlau (Chromoly) Kev xaiv siv hlau ua haujlwm yog ib qho zoo tshaj plaws ntawm kev sib tw tsheb thiab cov dav hlau uas nyiam tshaj plaws ntawm kev sib tw tsheb thiab cov dav hlau uas tau nyiam dua tshiab thaum ntxov xyoo pua 20th {7} {}
2. Puas muaj cov hlau chrome-molybdenum hlau zoo dua li cov hlau?
Dab tsi paub qhov txawv Chrome-Molybdenum hlau los ntawm lwm hom steel yog nws lub zog tshaj plaws tsis muaj kev sib tw lossis dej noo .
{{0 {}}} yuav 4130 chrome-molybdenum steel hlau xeb?
Ob qho tib si 4140 thiab 4130 tus hlau yog cov hlau loj uas muaj lub zog zoo, kev ua tsis tau zoo, thiab corrosion tsis kam {}}
{{04. yog 4130 ib cov roj carbon hlau?
4130 Cov hlau roj hmab yog cov siv roj carbon tsawg nrog kwv yees li ntawm cov steel thiab moly beld thiab moly beld thiab tuaj yeem kho cua sov yooj yim dua li lwm cov hlau me me.

Cim npe nrov: Alloy 4130 Steel Vuam Yeeb Nkab, Tuam Tshoj Alloy 4130 Steel Vuam Yeeb Yeeb Nkab

Xa kev nug

whatsapp

Xov tooj

Tug

Kev nug