Sep 26, 2025 Tso lus

UN tsis yog N06002 / h nr . 2.4665 sadalloy raj rau hastelloy x npib xee xeeloy

1. Dab tsi yog cov tshuaj lom neeg muaj pes tsawg leeg ntawm tsis ua N06002 (Hastelloy X)?

 

Teb:
Hastelloy X yog npib tsib xee - based supalloy. Nws cov ntawv muaj pes tsawg yog:

Nickel (NI): Tshuav (~ 47-55%)

Chromium (CR): 20-23%

Hlau (FE): 17% Max

Molybdenum (MO): 8-10%

Cobalt (CO): 1% Max

Cov ntsiab me: carbon, manganese, silicon, titanium, txhuas nyob rau hauv kab lw nyiaj

Qhov no muaj pes tsawg leeg muab kev ua tau zoo tshaj - kub lub zog thiab oxidation tsis kam.

 


2. Dab tsi yog cov khoom tseem ceeb ntawm hastelloy x leeg?

 

Teb:
Raug cov khoom ntawm chav tsev kub:

Lub zog tensile: ~ 758 mpa

Peple zog: ~ 310 mpa

Elongation: ~ 40%

Hardness: ~ 95 hrb

Nws muaj lub zog zoo, cov plhuav, thiab ductility ntawm kev nce siab kub txog ~ 1200℃f (650 degree).

 


3. Dab tsi yog thawj cov ntawv thov ntawm no superalloy raj hauv cov tshuab cua dav hlau?

 

Teb:
Hastelloy x leeg yog tsuas yog siv rau:

Combustor hnab looj thiab cov qauv txhawb nqa

Roj thiab Cua Txias Tubing Hauv Siab - kub seem

Cov khoom siv uas xav tau oxidation tsis kam thiab muaj zog hauv cov dav hlau xyaw

Nws qhov siab - kub oxidation tsis kam thiab corrosion tsis kam ua rau nws zoo tagnrho rau cov dav hlau cav ntoo.

 


4. Yuav ua li cas yuav tsum haastelloy x leeg yuav ua tiav lossis fabricated?

 

Teb:

Machining: tuaj yeem ua tau nrog carbide lossis coated cuab yeej; Lo Lus Txias Kom pom zoo vim ua haujlwm tawv.

Vuam: roj tungsten arc vuam (gtaw) lossis electron nqaj vuam vuam yog nyiam.

Kev Kho Cua Sov: Kev nyuaj siab nyem thaum 1175-1200 Qib F (635-650 degree) tuaj yeem txo cov kev ntxhov siab uas muaj kev ntxhov siab.

Kev tsim: Kev pom zoo kub yog pom zoo; Kev txias txias yog ua tau nrog kev saib xyuas vim ua haujlwm tawv.

 


5. Dab tsi yog qhov corrosion thiab oxidation tsis kam ntawm hastelloy x?

 

Teb:

Zoo heev rau oxidation thiab carburization nyob rau hauv huab cua lossis kev sib txuas ib puag ncig mus txog 1200℃f (650 degree).

Resistant rau chloride -} indive kev nyuaj siab corrosion.

Ua tau zoo nyob rau hauv acidic lossis hakide -} muaj cov cua txias ntawm cov dav hlau ib puag ncig.