Cov khoom siv yog dab tsi yog GH3039 Superalloy

1. Cov khoom siv twg yog GH3039 SuperSlloy?

GH3039 yog aNickel -} Raws li wrought wroughtThawj feem ntau tsim rau high - kev pab kub. Nws belongs rau cov khoom -} Kev daws teeb meem, thiab tungsten) rau hauv lub nroog tsibkel, es tsis txhob cia siab rau cov nag lossis daus.
Qhov no alloy ua pov thawj kev hloov kho zoo, suav nrog cov oxidation zoo tiv thaiv, thiab lub zog kub (feem ntau yuav mus txog800-900 degree). Nws tseem tswj hwm kev txaus siab thiab cov txheej txheem, ua rau nws siv dav hlau, thiab muaj kev lag luam {{{{2} kub ceev rau cov tshuab hluav taws xob thiab cov tshuab hluav taws xob.

2. Dab tsi yog cov tshuaj lom neeg muaj pes tsawg leeg ntawm Gh3039 SuperSlloy?

Cov tshuaj lom neeg muaj pes tsawg leeg ntawm Gh3039 yog nruj me ntsis tswj tau kom ntseeg tau nws qhov siab- kub ua tau zoo. Cov lus hauv qab no teev cov nominal muaj pes tsawg leeg (los ntawm qhov hnyav feem pua, wt%):
Lub ntsiab Cov ntsiab lus ntau (WT%) Rooj mov
Npib tsib caug (ni) Ntau dua los yog sib npaug rau 72.0 Matrix caij; Muab cov hauv paus muaj zog thiab ruaj khov ntawm qhov kub.
Chromium (cr) 19.0 – 22.0 Txhim kho oxidation thiab siab - kub corrosion tsis kam.
Molybdenum (mo) 2.0 – 3.0 Txhim kho cov khoom khov kho -} Kev daws teeb meem ntxiv thiab nkag mus.
Tungsten (w) 0.5 – 1.0 Pab cov khoom -}} kev daws teeb meem ntxiv thiab txhim kho siab- qhov kub thiab txias.
Hlau (FE) Tsawg dua los yog sib npaug rau 1.5 Txo tus nqi; muaj cov nyhuv me rau matrix stability.
Titanium (ti) 0.15 – 0.35 Nplua -} Tunes Landes qauv; Ua kom muaj zog me ntsis.
Aluminium (AL) 0.15 – 0.35 Ua cov yeeb yaj kiab ntom nti al₂o₃ oxide zaj duab xis; Txhim kho qhov siab - kub oxidation tsis kam.
Carbon (c) Tsawg dua los yog sib npaug rau 0.08 Txhim kho carbide tsim; Txhim kho cov coj tawm tsam (tswj kom tsis txhob muaj tus saib xyuas muaj tseeb carbides).
Manganese (mn) Tsawg dua los yog sib npaug rau 0.70 Txhim kho cov haujlwm kub.
Silicon (si) Tsawg dua los yog sib npaug rau 0.80 AIDS hauv DEEAGIDation thaum lub sijhawm smelting; txhim kho oxidation tsis kam.
Phosphorus (p) Tsawg dua los yog sib npaug rau 0.030 Impurity lub caij; nruj me ntsis txwv kom tsis txhob txo qis duas.
Sulphur (s) Tsawg dua los yog sib npaug rau 0.020 Impurity lub caij; nruj me ntsis txwv kom tiv thaiv kub brittleness.

info-440-447info-448-444

info-448-444info-445-446

3. Dab tsi yog qhov nyuaj ntawm Gh3039 SuperSlloy?

Lub hardness ntawm Gh3039 Superalloy tsis tas tsau; nws txawv tseem nyob ntawm nwsKev Kho Cua Sov Lub XeevthiabUa mob(piv txwv li, ua haujlwm txias). Hauv qab no yog cov kev ua kom nruj ib txwm rau cov xeev:

Annealed xeev: Qhov no yog lub xeev ntau tshaj plaws rau Gh3039, raws li anealing relieves sab hauv kev ntxhov siab thiab ua kom nruj kev ductility. Cov tawv tawv ib txwm yogHB 190 - 220(Brinell hardness) lossisHV 200 - 230(Vickers hardness).

Txias -} Ua haujlwm lub xeev: Tom qab ua haujlwm txias (piv txwv li, dov, kos duab), lub pob zeb alloy yog deformed, ua rau nce hardness. Lub hardness tuaj yeem sawvHB 250 - 300lossisHV 260 - 310, tab sis kev sib luag yuav txo qis kom haum.

High - kev pabcuam kub lub xeev: Thaum ua haujlwm kub (800-900 degree), lub hardness), lub hardness ntawm Gh3039 txo me ntsis vim yog softening, tab sis nws tseem tswj lub zog txaus rau kev tawm tsam hauv qab.

Nws yuav tsum tau sau tseg tias hardness ntsuas rau superalloys feem ntau yog ua raws li cov qauv xws li ASTM E10 (Brinell) lossis ASTM E92 (cov vickers) kom ntseeg tau qhov tseeb.