Nickel 200 (UNS N02200) thiab 201 (UNS N02201) yog ob daim ntawv pov thawj wrought nickel khoom. Lawv txawv tsuas yog nyob rau hauv cov ntsiab lus siab tshaj plaws carbon - 0.15% rau Nickel 200 thiab 0.02% rau Nickel 201.
Nickel 200 feem ntau txwv rau kev ua haujlwm ntawm qhov kub qis dua 600 degree F (315 degree) vim tias thaum kub siab dua nws yuav raug kev txom nyem los ntawm graphitization uas tuaj yeem ua rau cov khoom puas tsuaj loj heev. Thaum kub siab dua Nickel 201 yuav tsum tau siv. Ob chav kawm tau pom zoo rau ASME Boiler thiab Pressure Vessel Code, Tshooj VIII, Ntu 1. Nickel 200 tau pom zoo rau kev ua haujlwm kub txog 600 degree F (315 degree), thaum Nickel 201 tau pom zoo txog 1250 degree F (677 degree. ).


Ob qib qhia tau zoo heev tiv thaiv rau caustic soda corrosion thiab lwm yam alkalis. Cov khoom ntawm cov hlau no muaj txiaj ntsig zoo tshaj plaws hauv kev txo qis ib puag ncig, tab sis kuj tuaj yeem siv nyob rau hauv oxidizing tej yam kev mob los tsim ib tug passivating oxide zaj duab xis. Ob leeg tiv thaiv corrosion los ntawm distillation, dej ntuj thiab ntws seawater tab sis raug tawm tsam los ntawm cov dej hiav txwv stagnant.
Nickel 200 thiab 201 yog ferromagnetic thiab nthuav tawm cov ductility siab thiab ntau yam ntawm cov khoom siv kho tshuab tshaj qhov kub thiab txias. Ob qib yog yooj yim rau welding thiab tsim los ntawm cov txheej txheem khw fabrication.