Khoom Taw qhia
Incoloy 330 daim ntawv thov
▪ Kev lag luam cua sov
▪ Furnaces, muffles, rov ua haujlwm thiab conveyor tshuab
Kho cov pob tawb thiab kho kom zoo
Incoloy 330 Cov Lus Qhia Tshwj Xeeb
| Unrical n08330 | SAE AMS 5592 | SAE Ams 5716 | SAE J405 | SAE J412 |
| ASTM B 511 | ASTM B 512 | ASTM B 535 | ASTM B536 | ASTM B546 |
| ASTM B710 | ASME SB -511 | ASME SB -536 | ASME SB -710 |
Incoloy 330Tshuaj Muaj Tshuaj
| Lub ntsiab | Cov ntsiab lus (%) |
| Hlau, FE | 43 |
| Npib tsib xee, ni | 34-37 |
| Chromium, cr | 17-20 |
| Manganese, mn | Tsawg dua los yog sib npaug rau 2 |
| Lwm tus | Qho tseg |
Incoloy 330Cov Khoom Siv Neeg Kho Tshuab
| Cov Khoom Siv | Me me | Muaj huab tais |
| Lub zog tensile (annealed) | 600 MPa | 87 ksi |
| Yield zog (annealed) | 280 MPa | 40.6 Ksi |
| Elongation thaum so | 45% | 45% |
Kev Cai Rooj


Cim npe nrov: Ams 5716 / N08330 / ASTM B536 Superalalloy Sawb Rau Industracy Scoloy 330 Nickel Alloy Chev Cov Khoom Siv